Peculiarities of corrosion parameters for superalloy SLZhS5-VI



Full text article ( in russian)

Year

 
2017

Issue

 
382

Volume

 
4

Pages

 
113-116

Caption

 
Peculiarities of corrosion parameters for superalloy SLZhS5-VI .

Authors

 
Bagerman A., Konopatova A., Kirshin A., Neudakhina A., Danilov D.

Keywords

 
gas turbine, heat-resistant alloy, high-temperature corrosion, mass loss, salt load.

DOI

 
10.24937/2542-2324-2017-4-382-113-116

Summary

 
Object and purpose of research.The object of this study was monocrystallic alloy SLZhS5-VI marketed as resistant against heat and corrosion.
Subject matter and methodsThe materials for this study were the data of the corrosion tests performed in the atmosphere that simulated the one in the air-gas channel of marine gas turbine. The tests were performed on the gas dynamic test rig, and the gas flow was fed with sea salt.
Main resultsThe study yielded the mass loss relationships for the material, both in air (oxidation) and in the gas flow, in the conditions of high-temperature salt-induced corrosion. These relationships were obtained for the temperatures of 700, 800, 900, 930, 950 °С. The results have shown that both in the air and in the conditions of corrosion, SLZhS5-VI alloy demonstrates considerably lower mass losses at the temperature of above 900 °C, which is unusual. The results obtained at the temperature of 950 °С were confirmed by the additional tests at the temperature of 930 °С.
Conclusion.The results of this study can be used to design new materials, to assess other materials for the presence of this effect, to develop the coatings for gas turbine channel elements, as well as to assess the effects of heavy service upon the turbine

Rubrics

 
Ship powering and electric systems

Back to the list



 





 
Login:
Password:
Register
Forgot your password?


Last issues

All rights reserved © Krylov state research centre, 2017 — 2022


ISSN (print) 2542-2324 / ISSN (online) 2618-8244

Address: Moskovskoye shosse, 44, Saint-Petersburg, 196158

Phone: +7(812) 415-49-80